MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman DuraGrip™ 6830 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs extensive line of Melt-Processable Elastomers™. FDA compliant grades with very good elastomeric properties and, when needed, a soft touch feel. Available in a wide variety of hardnesses

Advantages

  • Soft Grips –When combined with rigid thermoplastic substrates, DuraGrip adds an ergonomic, soft feel that increases customer value in household products, appliances, personal care items, hand tools, sporting goods, and more.
  • Eye-Catching Color – Makes this product more attractive to the customers with easily colorable natural, translucent, and clear grades.
  • Faster Cycle Times – DuraGrip flows easily and molds with precision, enabling you to realize maximum throughput and profitability.

    • General purpose performance
    • FD-compliant applications
    • Bonding to polypropylene and polyethylene
    • Engineered thermoplastic bonding
    • Clear products
    • Bonding to nylon

    Information provided by Advanced Polymer Alloys

    Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D471
Viscosity 129000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
129000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30305 Sec; ASTM D2240
Tensile Strength at Break 4.38 MPa635 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
100% Modulus 1.05 MPa
@Strain 100 %
153 psi
@Strain 100 %
ASTM D412
Graves Tear Strength 14.2 kN/m
@Temperature 24.0 °C
81.0 pli
@Temperature 75.2 °F
Die C; ASTM D624
Compression Set 10 %
@Temperature 24.0 °C,
Time 79200 sec
10 %
@Temperature 75.2 °F,
Time 22.0 hour
ASTM D395
Tensile Set 5.0 %5.0 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -68.0 °C-90.4 °FASTM D746
 
Descriptive Properties
ColorN,B,C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer
Avient Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Barlog Plastics KEBAFLEX S 25 A.01 TPE-S, Shore A25, translucent
Barlog Plastics KEBAFLEX SG 25 A.1 TPE-S, Shore A25, natural

PAPA049 / 24116

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.