MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

JIS SKH2 Tungsten-Alloy High-Speed-Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel

Key Words: JIS G4403(83) SKH2, SKH 2, SKH-2; Comparable to AISI T1, UNS T12001
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.67 g/cc0.313 lb/in³(AISI T1)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 248<= 248Bar Forging Annealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.70 µm/m-°C5.39 µin/in-°F(AISI T1)
Thermal Conductivity 20.0 W/m-K139 BTU-in/hr-ft²-°F(AISI T1)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 540 - 595 °C1000 - 1100 °FTempering Temperature (AISI T1)
 1260 - 1300 °C2300 - 2370 °FHardening Temperature (AISI T1)
Annealing Temperature 870 - 900 °C1600 - 1650 °F(AISI T1)
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.73 - 0.83 %0.73 - 0.83 %
Chromium, Cr 3.8 - 4.5 %3.8 - 4.5 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe 73.1 - 77.7 %73.1 - 77.7 %As Balance
Manganese, Mn <= 0.40 %<= 0.40 %
Nickel, Ni <= 0.25 %<= 0.25 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.030 %<= 0.030 %
Tungsten, W 17.00 - 19.00 %17.00 - 19.00 %
Vanadium, V 0.80 - 1.2 %0.80 - 1.2 %
 
Descriptive Properties
Quench MediumO, A, S

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type T1 Tungsten-Alloy High-Speed-Tool Steel (UNS T12001)
Tungsten, W
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
CoCrMoWNi Alloy, ASTM F563
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy

MSTZJSKH2 / 231099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.