MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asian Jelutong Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Latex ducts may be present
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Permeable
Common Applications: Pattern making, drawing boards

Key Words: Dyera costulata; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.360 g/cc0.360 g/ccGreen
Density 0.470 g/cc0.0170 lb/in³15% Moisture Content
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1500 N337 lb (f)Side Hardness, Green
 1700 N382 lb (f)Side Hardness, 12% Moisture
Modulus of Rupture 0.0386 GPa5.60 ksiStatic Bending, Green
 0.0503 GPa7.30 ksiStatic Bending, 12% Moisture
Flexural Modulus 8.00 GPa1160 ksiStatic Bending, Green
 8.10 GPa1170 ksiStatic Bending, 12% Moisture
Compressive Strength 21.0 MPa3050 psiParallel to Grain, Green
 27.0 MPa3920 psiParallel to Grain, 12% Moisture
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 5.20 MPa754 psiParallel to Grain, Green
 5.80 MPa841 psiParallel to Grain, 12% Moisture
Work to Maximum Load 0.0390 J/cm³5.66 in-lb/in³Static Bending, Green
 0.0440 J/cm³6.38 in-lb/in³Static Bending, 12% Moisture
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.3 %2.3 %Radial Shrinkage Green to Oven Dry
 5.5 %5.5 %Tangential Shrinkage Green to Oven Dry
 7.8 %7.8 %Volumetric Shrinkage Green to Oven Dry
 
Descriptive Properties
ColorWhite to yellowUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asian Mengkulang Wood
Tropical Balsa Wood
Asian Kapur Wood
Asian Geronggang Wood
Asian Balau Wood

PTST380 / 71420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.