MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Integrate™ NP507030 Functionalized Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: INTEGRATE products are chemically modified polyolefins used to combine dissimilar materials for a variety of applications including molding articles, flexible materials and fiber technology or to provide property enhancements which fulfill final materials parameters. These products are particularly effective when the materials involved contain both polar and non-polar components. Specific ingredients may include polymers such as polyethylene and/or its copolymers, polypropylene and/or its copolymers, polyamides (nylons), polyacetates, cellulose, ionomers, polyethylene terephthalate (PET) resins and/or its copolymers as well as a variety of minerals, which can be used to improve strength or stiffness in the final composition. Individual product grades can be tailored for specific applications or properties. INTEGRATE products are available in pellet form. Contact your sales and/or Equistar technical service representative for more information and specific recommendations for your applications(s).

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D1505
Melt Flow 29 g/10 min
@Load 2.16 kg,
Temperature 230 °C
29 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Processing PropertiesMetricEnglishComments
Melt Temperature >= 204 °C>= 400 °FTo ensure adequate dispersion among components

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lushan M-20A Adhesive Resin for Multi-layer Oxygen Barrier Pipe
Mitsui ADMER® SF755A Elastomer Type Polyolefin
Mitsui ADMER® NF908A PE Type Polyolefin
Mitsui ADMER® AT2018A PE Type Polyolefin
LyondellBasell Plexar PX6002 Polyolefin

PEQU0699 / 37168

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.