MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wacker Powersil® 466 LV A/B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® 466 LV A/B is a liquid silicone rubber with medium conductivity and excellent mechanical properties.

Special features:

  • low viscosity liquid silicone rubber
  • high elongation at break, low tension set
  • stable electrical properties
  • good mechanical properties
  • ready-to-use, two-component system
  • suitable for cold shrink technology
Application: POWERSIL® 466 LV A/B is suitable for production of electrically conductive injection molded articles, especially cable accessories in the medium and high voltage range. The range of use spreads from push-on accessories to cold shrink applications. POWERSIL® 466 LV A/B combines a low Shore A Durometer with high elongation, good setting properties (low tension set) and good mechanical properties which are a must for cold shrink applications. POWERSIL® 466 LV A/B is a low viscosity

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183-1 A
Viscosity  350000 cP
@Shear Rate 10.0 1/s
350000 cP
@Shear Rate 10.0 1/s
Component B; ISO 3219
 400000 cP
@Shear Rate 10.0 1/s
400000 cP
@Shear Rate 10.0 1/s
Mix; ISO 3219
 450000 cP
@Shear Rate 10.0 1/s
450000 cP
@Shear Rate 10.0 1/s
Component A; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3232ISO 868
Tensile Strength at Break 6.00 MPa870 psiISO 37
Elongation at Break 670 %670 %ISO 37
100% Modulus 0.700 MPa
@Strain 100 %
102 psi
@Strain 100 %
ISO 37
300% Modulus 2.30 MPa
@Strain 300 %
334 psi
@Strain 300 %
ISO 37
Tear Strength 22.0 kN/m126 pliASTM 624 B
Compression Set 11 %11 %
Tensile Set <= 5.0 %<= 5.0 %ISO 2285
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 40 ohm-cm40 ohm-cmASTM D991
 50 ohm-cm50 ohm-cmIEC 60093
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
post-cured for 4h at 200°C
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vicone High Performance Rubber VicoSil™ C306E-GR High Performance Silicone Rubber
Vicone High Performance Rubber VicoSil™ C303Q-GY High Performance Silicone Rubber
Trelleborg S650 Silicone Rubber
Shin-Etsu Silicones LIMS™ KE1950-35A/B Elastomer
Shin-Etsu Silicones LIMS™ KE1950-30A/B Elastomer

PWACK9372 / 204901

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.