MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beijing Evergrow Resources CFC-DDX-1000S Carbon Fiber Cloth
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corrosion resistance for many kinds of organic solvents, it is widely used in military,aerospace fields, and also as electric conductive and exothermic materials used in many industrial fields.

    Applications:
  • Military, aerospace industry
  • Electric conductive and exothermic materials

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 - 1.62 g/cc0.0578 - 0.0585 lb/in³
Thickness 120 - 200 microns4.72 - 7.87 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 250 MPa>= 36300 psiweft
 >= 350 MPa>= 50800 psiwarp
 
Component Elements PropertiesMetricEnglishComments
Carbon, C >= 90 %>= 90 %
 
Descriptive Properties
Conductivity (ohms/20mm)10-20, 15-25
Weavetwill
Weight (g/m²)145-175
Width (mm)950-1050

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DowAksa AKSACA™ A-49 D 24K Continuous Carbon Fiber
Beijing Evergrow Resources Carbon Fiber Felt
Beijing Evergrow Resources CFC-DD-1000 Carbon Fiber Cloth
Beijing Evergrow Resources CFC-DDX-1000 Carbon Fiber Cloth
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2

PBEIJ055 / 90124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.