MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Eastalloy MA510 Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhanced physical properties advantages.

Applications/Uses

  • Medical
  • Medical Devices
  • Key Attributes

  • Good chemical resistance
  • Good Clarity
  • Sterilizable with ethylene oxide, electron beam, and gamma rays
  • Wide range of clear tints and opaque colors
  • Elevated in-use temperature resistance
  • Heat resistance
  • Tough, excellent impact strength

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
    Water Absorption 0.15 %0.15 %24h Immersion; ASTM D570
    Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break 56.0 MPa8120 psiASTM D638
    Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
    Elongation at Break 195 %195 %ASTM D638
    Elongation at Yield 5.5 %5.5 %ASTM D638
    Flexural Strength 76.0 MPa11000 psiASTM D790
    Flexural Modulus 2.10 GPa305 ksiASTM D790
    Izod Impact, Notched  0.910 J/cm
    @Temperature -40.0 °C
    1.70 ft-lb/in
    @Temperature -40.0 °F
    ASTM D256
     NB
    @Temperature 23.0 °C
    NB
    @Temperature 73.4 °F
    ASTM D256
    Izod Impact, Unnotched NBNBASTM D4812
     NB
    @Temperature -40.0 °C
    NB
    @Temperature -40.0 °F
    ASTM D4812
    Puncture Energy 55.0 J40.6 ft-lbPuncture Resistance @Max Load, 23°C; ASTM D3763
     49.0 J
    @Temperature -40.0 °C
    36.1 ft-lb
    @Temperature -40.0 °F
    Puncture Resistance at Max Load; ASTM D3763
     
    Thermal PropertiesMetricEnglishComments
    Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °FASTM D648
     
    Optical PropertiesMetricEnglishComments
    Haze 0.50 %0.50 %ASTM D1003
    Transmission, Visible 86 %86 %Total Transmittance; ASTM D1003
     
    Processing PropertiesMetricEnglishComments
    Melt Temperature 266 - 288 °C511 - 550 °F
    Mold Temperature 27.0 - 60.0 °C80.6 - 140 °F
    Drying Temperature 88.0 °C190 °F
    Dry Time 4 - 6 hour4 - 6 hour

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Eastman Eastar GN002 Copolyester, Natural
    Eastman Eastar GN046 Copolyester, Natural
    Eastman Eastar GN078 Copolyester, Natural
    Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend
    Eastman Aqua PJ003 PET

    PE9018 / 35074

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.