MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tabriz LL 0410AA Low Density Polyethylene copolymer
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: LL0410AA is linear low density polyethylene copolymer containing butene-1(C4) as comonomer. It is suitable for blending with conventional LDPE. Film made from pure LL0410AA has the following advantages over LDPE: better sealing, lower seal shrinkage, greater drowdown ability and higher stiffness & toughness. Applications: green house film, silage film, hand bags and general purpose film applications.

Information provided by Tabriz Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D1505
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.0 MPa1740 psiASTM D882
Film Tensile Strength at Yield, TD 13.0 MPa1890 psiASTM D882
Film Elongation at Break, MD 620 %620 %ASTM D882
Film Elongation at Break, TD 850 %850 %ASTM D882
Dart Drop Test 80.0 g0.176 lbASTM D1709, method A
Film Tensile Strength at Break, MD 42.0 MPa6090 psiASTM D882
Film Tensile Strength at Break, TD 33.0 MPa4790 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 107 °C225 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Gloss 50 %50 %at 45°; ASTM D 2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® LB Polyester Film, 92 Gauge (23 µm)
ExxonMobil LL 6100 Injection Molding Resin
ExxonMobil C4LL 20025.17 Linear Low Density Polyethylene Resin
ExxonMobil C4LL 1018.76 Linear Low Density Polyethylene Resin
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer

PTABRZ913 / 198224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.