MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOM® MED PS 1000 AS 14115 Polystyrene, Impact
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Base Polymer: Polystyrene, impact

Filler/Additive System: antistatic-permanent

Special Features: Impact modified

Market Segment: Medical/Personal Care

Application Area: injection molded parts

Typical Applications: housings

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
@Time 86400 sec
0.0030 - 0.0050 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 17 g/10 min
@Load 5.00 kg,
Temperature 200 °C
17 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.0 MPa3770 psiISO 527
Elongation at Break 15 %15 %ISO 527
Elongation at Yield 1.3 %1.3 %ISO 527
Tensile Modulus 2.20 GPa319 ksiISO 527
Flexural Strength 40.0 MPa
@Strain 3.5 %
5800 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 2.10 GPa305 ksiISO 178
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -40.0 °C
21.4 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.200 J/cm²
@Temperature -40.0 °C
0.952 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C165 °FISO 75-1/-2
Vicat Softening Point 80.0 °C176 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 260 °C356 - 500 °FInjection molding
Mold Temperature 10.0 - 70.0 °C50.0 - 158 °FInjection molding
Drying Temperature  60.0 - 80.0 °C
@Time 7200 - 10800 sec
140 - 176 °F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
 60.0 - 80.0 °C
@Time 7200 - 10800 sec
140 - 176 °F
@Time 2.00 - 3.00 hour
in air circulating dryer
 
Descriptive Properties
Base PolymerPolystyrene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Aclo Accucomp Polystyrene HS0600L High Impact
API Megol AM SV/P SEBS Adhesion Modified Overmolding for Polar Polymers
Chi Mei Polyrex® PH-60 Polystyrene - High Impact
Total Lacqrene® 1235 High Impact Polystyrene

PALBIS8079 / 242138

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.