MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsui HILET™ 1351D Porous Polyethylene Membrane  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE)

Material Notes: HILET™ Porous Membrane is a polymeric membrane derived from ultra molecular weight polyethylene HI-ZEX® MILLION. Designed using a solvent poriferous procedure pioneered by Mitsui Chemicals, Inc., the company developed a low gauge polymeric membrane of high porosity and narrow pore size distribution without the use of organic fillers. HILET features high permeability and therefore low flow resistance during filtration and separation. In addition, the material retained the chemically stable properties of Polyethylene, so it has a low melting point to facilitate the closure of pores and reduction of flow through at elevated temperatures.

Available in sheet form, each sheet has a homogenous, three-dimensional structure (uniform pore size and distribution) with biaxial orientation. The film is relatively thin in consistency measuring about 1 mil in thickness with apertures ranging in size from 0.5 to 1 micron meters. HILET's property characteristics include:

  • High tensile strength
  • High flux and selectivity
  • Superb vapor permeability for greater media storage and longer filter life
  • Superior organic solvent, acid and water resistance
  • Excellent anti-friction and corrosion resistance
  • High durability and strong temperature tolerance yielding a low shrinkage ratio

Applications:

  • Enzyme harvesting in the biotechnology sector
  • Hemodialysis, drug detoxification and treatment of acute renal failure and liver and kidney functions in the medical arena
  • Removal of impurities in the food and beverage industry
  • Clean up of latex waste in the industrial water waste
  • Purification of drinking water
  • Removal of non biodegradable pollutants in the paper industry
  • Fuel cell proton exchange membrane material
  • Packing material for humidifiers

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.357 g/cc0.0129 lb/in³Calculated from Weight of 12.5 G/m2
Porosity 63 %63 %Void Content
Thickness 35.0 microns1.38 mil
Pore Size 0.0710 microns0.00280 milMean flow; ASTM Test
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 45 %45 %
Film Elongation at Break, TD 120 %120 %
Film Tensile Strength at Break, MD 65.0 MPa9430 psi
Film Tensile Strength at Break, TD 30.0 MPa4350 psi
 
Descriptive Properties
Air Resistance180 sec/100mlGurley, JIS
Piercing Strength400 G f

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
99.5% Alumina, porous body
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Mitsui HILET™ 2221 Porous Polyethylene Membrane
Momentive Performance Materials HTR1001 PBN/PG Heating Element
Separator material

PMIT052 / 53233

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.