MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Paper Birch Wood
Categories: Wood and Natural Products; Wood; Hardwood

Key Words: Betula Papyrifera; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.480 g/cc0.480 g/ccGreen, based on volume
 0.550 g/cc0.550 g/cc12% moisture content, based on volume
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2491 N560.0 lb (f)Green
 4048 N910.0 lb (f)12% moisture content
Tensile Strength at Break 2.62 MPa380 psiGreen, perpendicular to grain
Modulus of Elasticity 8.07 GPa1170 ksiGreen
 11.0 GPa1590 ksi12% moisture content
Modulus of Rupture 0.0441 GPa6.40 ksiGreen
 0.0848 GPa12.3 ksi12% moisture content
Compressive Strength 1.86 MPa270 psiGreen, perpendicular to grain
 4.14 MPa600 psi12% moisture content, perpendicular to grain
 16.3 MPa2360 psiGreen, parallel to grain
 39.2 MPa5690 psi12% moisture content, parallel to grain
Shear Strength 5.79 MPa840 psiGreen, parallel to grain
 8.34 MPa1210 psi12% moisture content, parallel to grain
Impact 3434Impact bending in inches, 12% moisture content
 4949Impact bending in inches, green
Work to Maximum Load 0.110 J/cm³16.0 in-lb/in³12% moisture content
 0.112 J/cm³16.2 in-lb/in³Green
 
Thermal PropertiesMetricEnglishComments
Shrinkage 6.3 %6.3 %Radial, from green to oven dry, US origin
 8.6 %8.6 %Tangential, from green to oven dry, US origin
 16.2 %16.2 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Yellow Birch Wood
Sweet Birch Wood
Black Maple Wood
American Maple, Rock (Sugar Maple)
Bigleaf Maple Wood

PTSU016 / 71458

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.