MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SGL Carbon Group PANOX® FA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX is ideal for processing into yarns, woven fabrics, nonwovens and felts.

Information provided by SGL Carbon Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 - 1.43 g/cc0.0502 - 0.0517 lb/in³Fiber Density
Filament Diameter 13 µm13 µm
Fiber Count 1.67 dtex1.50 denier
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psi
Elongation at Break 15 - 27 %15 - 27 %
Tenacity >= 0.140 N/tex>= 1.59 g/denier
 
Descriptive Properties
Typical Finish Content, %0.6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SGL Carbon Group PANOX® FA C063 EEA High performance Crimped staple oxidized textile fiber, For carbon/carbon and spinning
SGL Carbon Group PANOX® FB T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning
SGL Carbon Group PANOX® FA C063 SSC High performance Crimped staple oxidized textile fiber, For felts and non-wovens
Graphite, Carbon, C
SGL Carbon Group SIGRAFIL C® C25 S012 EPY Staple Carbon Fiber, Epoxy Sizing

ESGL11 / 5720

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.