MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Reliance Industries Relene B56003 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Relene B56003 is a High Density Polyethylene grade suitable for general purpose extrusion blow molding applications. Articles blown from this grade exhibit good stiffness. The resin offers good melt strength, ESCR and impact resistance and typically is used for packing of oils, vanaspati, and general purpose containers.

Information provided by Reliance Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³ASTM D1505
Melt Flow 0.30 g/10 min
@Load 2.16 kg
0.30 g/10 min
@Load 4.76 lb
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969ASTM D2240
Tensile Strength, Yield 26.0 MPa3770 psiASTM D638
Elongation at Break 550 %550 %ASTM D638
Flexural Yield Strength 28.5 MPa4130 psiASTM D790
Flexural Modulus 0.900 GPa131 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 128 °C262 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 175 - 205 °C347 - 401 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Reliance Industries Reclair F18010 Polyethylene
Reliance Industries Reclair M26500 Polyethylene
Reliance Industries Reclair M24300 Polyethylene
Reliance Industries Relene B31101 Polyethylene
Reliance Industries Reclair O21010 Polyethylene

PREL070 / 65410

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.