MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Karina 70900-35/1-E-AC Ivory PVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: Flame retardant PVC compound, class 70C (PVC/A), recommended for insulation of electrical wires and cables (BWF).

Information provided by Karina Indústria e Comércio de Plásticos Ltda.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 - 1.51 g/cc1.45 - 1.51 g/ccNBR NM-IEC 60811-1-3
ASTM Color -2.35 - 3.65-2.35 - 3.65Color A, ME 12
 3.66 - 9.663.66 - 9.66Color B, ME 12
 85.06 - 91.0685.06 - 91.06Color L, ME 12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 90 - 94
@Time 15.0 sec
90 - 94
@Time 0.00417 hour
NBR 7456
Tensile Strength >= 12.6 MPa>= 1820 psiNBR NM-IEC 60811-1-1
 >= 12.6 MPa>= 1820 psiAfter 168H in air oven at 100°C; NBR NM-IEC 60811-1-2
Elongation at Break >= 150 %>= 150 %NBR NM-IEC 60811-1-1
 >= 150 %>= 150 %After 168H in air oven at 100°C; NBR NM-IEC 60811-1-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 3.00e+14 ohm-cm>= 3.00e+14 ohm-cmNBR 5403
 
Thermal PropertiesMetricEnglishComments
Oxygen Index >= 30 %>= 30 %NBR 6245
 
Descriptive Properties
ApplicationGeneral Purpose Profiles
Maximum Variation of Elongation (%)25NBR NM-60811-1-2
Maximum Variation of Tensile Strength (%)25NBR NM-IEC 60811-1-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Karina E 72/206-IS Crystal PVC Compound (SP32811)
Karina E 65/225 Compound PVC Crystal
Karina E 90/212-DA-IS-SI-AT Compound PVC Crystal
Karina E 85/253-IS-SI-AT Compound PVC Crystal
Karina E 85/201-DA-IS-SI-AT Clear Crystal PVC Compound

PKARIN9346 / 171002

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.