Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, with mechanical properties that classify it as an engineering thermoplastic. This grade shows a unique balance of toughness and high modulus combined with good creep performance, strength and elevated temperature performance. Moreover this polymer exhibits a high resistance to hydrocarbons, solvents, salt solutions, weak acids and weak bases.
CARILON Polymer DB6G6A10 is easy to process on standard injection molding equipment. Cycle times are generally short and parts show good mold definition. CARILON Polymers' low moisture sensitivity means that no conditioning of parts before assembly or use is necessary. Data provided by Shell Chemical. |