MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals Novapol® HB-W952-A HDPE Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, high rigidity.

Applications: large-part blow-molding, trash cans, drums, jerry cans, fuel tanks.

Data provided by the manufacturer.

Key Words: High Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D792
Environmental Stress Crack Resistance 1000 hour1000 hourCondition A, 20% Igepal
ESCR 100% Igepal® >= 1000 hour>= 1000 hourF50, Condition B, ASTM D1693
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psiASTM D638
Elongation at Break 820 %820 %ASTM D638
Flexural Modulus 1.28 GPa186 ksiASTM D790
Izod Impact, Notched 3.90 J/cm7.31 ft-lb/inNotched/Unnotched not specified; ASTM D256
Tensile Impact Strength 320 kJ/m²152 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -100 °C<= -148 °FASTM D696
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Chevron Phillips Marlex® C513UV High Density Polyethylene, Blow Molding
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
NOVA Chemicals Novapol® HB-W747-A HDPE Extrusion Resin
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin

PEHN2O / 35609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.