MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Buckeye Polymers BP RPP 3009 GKW Polypropylene, Glass Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced engineering thermoplastics in numerous applications.

    Product Features:
  • Chemically coupled
  • Good flexural strength
  • Appearance: White

    Forms: Pellets

    Processing Method: Injection Moulding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 - 1.15 g/cc1.11 - 1.15 g/ccASTM D792
Ash 26 - 32 %26 - 32 %ASTM D5630
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 65.5 MPa>= 9500 psiASTM D638
Flexural Modulus >= 4.83 GPa>= 700 ksiASTM D790
Izod Impact, Notched >= 0.641 J/cm>= 1.20 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Buckeye Polymers BP RPP 3009 GK3 BLK Polypropylene, Glass Filled
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced
Buckeye Polymers BP RPP 3005 GR BLK Polypropylene, Glass Filled
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 20% Glass Fiber Filler

PBUCK015 / 104483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.