MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Duranex® 3105 Polybutylene Terephthalate (PBT), Standard, 15% GF filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers or other inorganic filler additives. Various grades are available, including flame-retardant, reinforced, and impact-resistant grades.

DURANEX®, due to its mechanical strength, heat stability, electrical resistivity and wear and abrasion-resistance, offers great potential as a well-balanced, highly reliable material, having a wide variety of applications including electronic / electro-mechanical and automobile parts and various other functional parts. DURANEX® also assures moldability, dimensional stability, glossy surfaces and various fabrication capabilities providing higher added value.

Information provided by PolyPlastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Filler Content 15 %15 %Glass fiber
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 105 MPa15200 psiISO 527-1, 2
Elongation at Break 2.5 %2.5 %ISO 527-1, 2
Flexural Strength 160 MPa23200 psiISO 178
Flexural Modulus 5.33 GPa773 ksiISO 178
Charpy Impact, Notched 0.580 J/cm²2.76 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cmIEC 60093
Surface Resistance 9.00e+15 ohm9.00e+15 ohmIEC 60093
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
22.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 207 °C405 °FISO 75-1, 2
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duranex® 304SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled
Polyplastics Duranex® 3400 Polybutylene Terephthalate (PBT), Standard, 40% GF filled
Polyram RamSter PF321G3 PBT, 15% Glass Fiber, Flame Retardant
Polyplastics Duranex® C5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled
Polyplastics Duranex® 3105H Polybutylene Terephthalate (PBT), Standard, 15% GF filled

PPOLPL050 / 57043

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.