MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Techical Ceramics MYCROSINT® SO 20 Boron Nitride
Categories: Ceramic; Carbide

Material Notes:

Information provided by 3M Technical Ceramics, formerly ESK Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 2.30 g/cc>= 0.0831 lb/in³Anisotropic, Perpendicular; DIN EN 623-2
 >= 2.30 g/cc>= 0.0831 lb/in³Anisotropic, Parallel; DIN EN 623-2
Porosity <= 10 %<= 10 %Anisotropic, Perpendicular; DIN EN 623-2
 <= 10 %<= 10 %Anisotropic, Parallel; DIN EN 623-2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 3030Anisotropic, Perpendicular; DIN EN ISO 6506-1
 3030Anisotropic, Parallel; DIN EN ISO 6506-1
Tensile Modulus 20.0 GPa2900 ksiYoung's, Anisotropic, Parallel; DIN EN 843-2
 35.0 GPa5080 ksiYoung's, Anisotropic, Perpendicular; DIN EN 843-2
Flexural Strength 40.0 MPa5800 psiAnisotropic, Parallel; DIN EN 843-1
 70.0 MPa10200 psiAnisotropic, Perpendicular; DIN EN 843-1
Compressive Strength 85.0 MPa12300 psiAnisotropic, Perpendicular; AAW/AC-R-302-03
 100 MPa14500 psiAnisotropic, Parallel; AAW/AC-R-302-03
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmAnisotropic, Perpendicular
 >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmAnisotropic, Parallel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.500 µm/m-°C
@Temperature 20.0 - 500 °C
0.278 µin/in-°F
@Temperature 68.0 - 932 °F
Anisotropic, Perpendicular; DIN EN 821-1
 0.500 µm/m-°C
@Temperature 1000 - 1500 °C
0.278 µin/in-°F
@Temperature 1830 - 2730 °F
Anisotropic, Perpendicular; DIN EN 821-1
 1.90 µm/m-°C
@Temperature 500 - 1000 °C
1.06 µin/in-°F
@Temperature 932 - 1830 °F
Anisotropic, Perpendicular; DIN EN 821-1
 2.20 µm/m-°C
@Temperature 1000 - 1500 °C
1.22 µin/in-°F
@Temperature 1830 - 2730 °F
Anisotropic, Parallel; DIN EN 821-1
 4.60 µm/m-°C
@Temperature 20.0 - 500 °C
2.56 µin/in-°F
@Temperature 68.0 - 932 °F
Anisotropic, Parallel; DIN EN 821-1
 6.60 µm/m-°C
@Temperature 500 - 1000 °C
3.67 µin/in-°F
@Temperature 932 - 1830 °F
Anisotropic, Parallel; DIN EN 821-1
Specific Heat Capacity 0.600 J/g-°C0.143 BTU/lb-°FAnisotropic, Perpendicular
 0.600 J/g-°C0.143 BTU/lb-°FAnisotropic, Parallel
Thermal Conductivity 25.0 W/m-K174 BTU-in/hr-ft²-°FAnisotropic, Parallel
 45.0 W/m-K312 BTU-in/hr-ft²-°FAnisotropic, Perpendicular
Maximum Service Temperature, Air 1100 °C2010 °FOxidizing, Anisotropic, Perpendicular
 1100 °C2010 °FOxidizing, Anisotropic, Parallel
Maximum Service Temperature, Inert 1800 °C3270 °FAnisotropic, Perpendicular
 1800 °C3270 °FAnisotropic, Parallel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Techical Ceramics MYCROSINT® HD Boron Nitride
3M Techical Ceramics MYCROSINT® CD Boron Nitride
3M Techical Ceramics MYCROSINT® S Boron Nitride
3M Techical Ceramics MYCROSINT® SO 43 Boron Nitride
3M Techical Ceramics MYCROSINT® O 40 Boron Nitride

CESK17 / 183309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.