MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solving problems associated with build-up of electrostatic charges, electrostatic discharge, and electromagnetic interference. These materials span the surface resistivity spectrum from antistatic through conductive to EMI shielding (100-1012O).

Applications: I.C. tray, wafer carrier, I.C. magazine, notebook PC case, home appliance part, LCD cassette tray

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength at Break 142 MPa20600 psiASTM D638
Elongation at Break <= 10 %<= 10 %ASTM D638
Flexural Strength 196 MPa28400 psiASTM D790
Flexural Modulus 9.81 GPa1420 ksiASTM D790
Izod Impact, Notched 0.490 J/cm0.918 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm - 1e+0510000 ohm-cm - 1e+05ASTM D257
Surface Resistance 10000 ohm - 1e+0510000 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity >= 0.270 W/m-K>= 1.87 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 300 °C500 - 572 °F
Middle Barrel Temperature 270 - 320 °C518 - 608 °F
Front Barrel Temperature 275 - 320 °C527 - 608 °F
Nozzle Temperature 275 - 320 °C527 - 608 °F
Melt Temperature 280 - 320 °C536 - 608 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 120 °C248 °F
Dry Time 4 hour4 hour
Injection Pressure 49.03 - 78.45 MPa7111 - 11380 psiSecond
 68.65 - 88.26 MPa9957 - 12800 psiFirst
Back Pressure 0.000 - 1.96 MPa0.000 - 284 psi
Screw Speed 40 - 60 rpm40 - 60 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Global EPP PA 6C Cast Polyamide 6
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic

PLGCHEM128 / 50949

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.