MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® OL22 Polyester Film, 100 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Product Description: Mylar® OL22 is a one side heat sealable, polyester film. It can be heat sealed to itself and heat seals well to thermoformed APET/CPET trays and APET coated board. It also heat seals to various other substrates including PVdC, PVC, paper and aluminum foil, but will not seal to polyolefins. The plain or non-heat seal surface of Mylar® OL22 exhibits the properties of standard polyester film.

General Product Info: Mylar® OL22 has an exceptionally wide heat seal range, from 220°F to 400°F, with outstanding hot tack properties. The plain surface of Mylar® OL22 can be printed or metallized in the same way as plain polyester film, although the sealable surface makes handling of the film during conversion more critical. The heat seal surface of the film is normally wound on the inside of the roll.

Typical Applications: Mylar® OL22 is an excellent film for applications where chemical resistance of the sealant surface is required. It offers excellent thermal properties in freezer to oven applications for lidding applications.

Approvals: FDA Food Contact Status - All gauges of Mylar® OL22 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Mylar® OL22 can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³Typical Mylar®; ASTM D1505
Water Vapor Transmission 17.1 g/m²/day
@Temperature 38.0 °C
1.10 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM F1249
Thickness 25.4 microns1.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 100 %100 %ASTM D882A
Film Elongation at Break, TD 90 %90 %ASTM D882A
Coefficient of Friction, Dynamic 0.500.50ASTM D1894
Film Tensile Strength at Break, MD 186 MPa27000 psiASTM D882A
Film Tensile Strength at Break, TD 200 MPa29000 psiASTM D882A
Heat Seal Strength 500 g/25 mm
@Time 1.00 sec
1.10 lb/in
@Time 0.000278 hour
285°C (HS/HS)
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Shrinkage, MD 3.5 %
@Temperature 190 °C,
Time 300 sec
3.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
1.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.64 - 1.671.64 - 1.67typical of Mylar®
Haze 6.0 %6.0 %ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)3.1 cc/100 in2O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal)16500 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge
DuPont Teijin Films Mylar® MLB Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® OB13AF Polyester Film, 100 Gauge

PDTZ9387 / 139707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.