MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aperam Nicrimphy® 600 Cold Rolled Strip
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Nicrimphy 600 is a nickel chromium alloy designed to offer good corrosion and oxidation resistance. It has also good mechanical properties over a wide range of temperatures. Nicrimphy 600 is used for: automotive industry (airbag components, heat screens, gaskets, exhaust systems..), muffles, furnace components, heating elements, aircraft industry, chemical industry, food and pharmaceuticals industries.

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.43 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 160160Annealed
Tensile Strength 650 MPa94300 psiAnnealed
Tensile Strength, Yield 300 MPa43500 psiAnnealed
Elongation at Break 35 %35 %Annealed
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000103 ohm-cm0.000103 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.3 µm/m-°C
@Temperature 20.0 - 100 °C
7.39 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity 14.7 W/m-K102 BTU-in/hr-ft²-°F
Melting Point 1370 °C2500 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 14 - 17 %14 - 17 %
Iron, Fe 6.0 - 10 %6.0 - 10 %
Nickel, Ni >= 72 %>= 72 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Nucalloy® 41 Nickel-Chromium-Boron Alloy
H.C. Starck Ni-SA 625 Nickel Super Alloy
Aperam Resistohm® 80 Resistant Alloys-Nickel Chromium Alloys
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes 214® Alloy Sheet

NPERA034 / 194823

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.