MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accutech Polypropylene Copolymer CP0436T20L1 Talc Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inMD; ASTM D955
Melt Flow 12 g/10 min12 g/10 minASTM D1238
Ash 20 %20 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6060ASTM D785
Tensile Strength at Break 18.0 MPa2610 psiASTM D638
Tensile Strength, Yield 23.0 MPa3340 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Tensile Modulus 1.80 GPa261 ksiASTM D638
Flexural Strength 31.0 MPa4500 psiASTM D790
Flexural Modulus 1.80 GPa261 ksiASTM D790
Izod Impact, Notched 0.747 J/cm1.40 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C136 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Homopolymer HP0334T20L Talc Reinforced
Aclo Accuguard Polypropylene CP0467V0CSV Copolymer Flame Retardant Automotive Approved grade
Aclo Accutech Polypropylene HP0335T40V Homopolymer Talc Reinforced
Bamberger Polymers Bapolene® 4042 Polypropylene, Fiber/Filament Grade
TIMCAL TIMREX® PP 10 Natural Flake Graphite

PACLO228 / 22483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.