MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CIMBAR Gel Talc for Polyester Filler
Categories: Ceramic; Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyester compounds where consistent viscosity is critical and inherent low oil absorption provides higher filler loadings. Gel Talc and Body Filler talcs are platy, hydrophobic and non-abrasive.
Gel Talc is specifically designed for gel coats where excellent color, predictable viscosity and superior surface characteristics are required.

Information provided by Cimbar Performance Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.78 g/cc2.78 g/cc
Bulk Density 0.368 g/cc0.0133 lb/in³Loose
 0.961 g/cc0.0347 lb/in³Tapped
Brightness 92 %92 %Hunter Y, Rd value, dry
Oil Absorption 26 %26 %g oil/100 g filler; ASTM D281
Fineness 5.05.0Hegman Fineness; ASTM D1210
Moisture Absorption at Equilibrium <= 0.30 %<= 0.30 %
Loss On Ignition 17 %17 %
Particle Size 1.0 µm1.0 µm@ 10%
 5.5 µm5.5 µmD50
 27 µm27 µm@ 98%
pH 9.09.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 1.01.0
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.571.57
 
Component Elements PropertiesMetricEnglishComments
Al2O3 <= 1.0 %<= 1.0 %
CaO <= 13 %<= 13 %
Fe2O3 <= 1.0 %<= 1.0 %
MgO 24 %24 %
SiO2 46 %46 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CIMBAR RP 9405 Talc
CIMBAR RP 9305 Talc
CIMBAR RP 9410 Talc
CIMBAR CIMTUFF® 9102 Talc
CIMBAR EliteTalc® 20 Cosmetic Talc

CIMBAR943 / 133425

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.