MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

China-Yixing Longly Refractories Tube SiC
Categories: Ceramic; Carbide

Material Notes: SiC tube made by our company have lots of superior performance, such as high refractoriness, good wear and corrosion resistance, hardness, strength, thermal conductivity, thermal shock stability, as well as good oxidation resistance. Inside diameter and outside diameter size can be based on the need for users to design process.

Applications: Widely used in a variety of heat treatment furnace, metallurgical sintering furnace, as well as IF forging furnace, smelting of nonferrous metals and chemical industries.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.55 - 2.70 g/cc0.0921 - 0.0975 lb/in³
Porosity <= 20 %<= 20 %Apparent
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength >= 450 MPa>= 65300 psicold bending
 >= 480 MPa>= 69600 psihigh temp bending
Compressive Strength >= 430 MPa>= 62400 psiAmbient
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.00 µm/m-°C1.67 µin/in-°FVolumetric thermal expansion
Thermal Conductivity 18.5 - 20.2 W/m-K128 - 140 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air >= 1450 °C>= 2640 °F
 
Component Elements PropertiesMetricEnglishComments
SiC 80 - 85 %80 - 85 %
 
Descriptive Properties
Refractoriness (°C)>1400Under load temperature, 0.2 MPa, 0.6%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories SBSN-CT Tube
Oxygen-free extra-low phosphorus Copper, UNS C10300, H80 (15%) temper, tube, shapes
Pyrotek MC-1 Metal Ceramic Thermocouple Protection Tube
Oxygen-free extra-low phosphorus Copper, UNS C10300, OS025 temper, flat products, tube
Chosun Refractories SSBA Tube

CYXLR014 / 99316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.