MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Starflex® GM1210BE Metallocene Linear Low Density Polyethylene, Film Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Starflex GM1210BE is a pelletized mLLDPE resin for use in applications that require maximum strength and toughness. GM1210BE contains a processing aid, slip and antiblock.

GM1210BE meets the requirements of the Food and Drug Administration 21 CFR 177.1520. This regulation allows for, among other things, the use of this olefin polymer in” …articles or components or articles intended for use in contact with food.” Certain limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Recommended processing conditions for GM1210BE are a 400° - 450°F melt temperature and a 1.5 to 3.0 blow-up ratio. Using proper techniques, these products can readily be drawn below 0.9 mils at optimum production rates. Specific recommendations for type of mLLDPE resin and extrusion conditions can only be made when the end use, required properties and extrusion equipment are provided; however, Equistar recommends that users conduct performance testing on finished articles in order to make an independent determination that GM1210BE is suitable and safe for all intended uses and applications.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.912 g/cc0.0329 lb/in³base resin; ASTM D1505
 0.916 g/cc0.0331 lb/in³ASTM D1505
Thickness 19.0 microns0.750 mil
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 5000 ppm5000 ppm
Slip Level 1000 ppm1000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 400 %400 %ASTM D882
Film Elongation at Break, TD 500 %500 %ASTM D882
Elmendorf Tear Strength MD 140 g140 gASTM D1922
Elmendorf Tear Strength TD 200 g200 gASTM D1922
Dart Drop 31.5 g/micron800 g/milASTM D4272
Film Tensile Strength at Break, MD 65.5 MPa9500 psiASTM D882
Film Tensile Strength at Break, TD 42.7 MPa6200 psiASTM D882
1% Secant Modulus, MD 152 MPa22000 psiASTM D882
1% Secant Modulus, TD 159 MPa23000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 16 %16 %ASTM D1003
Gloss 45 %45 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 232 °C400 - 450 °F
Blow-up Ratio (BUR) 2.52.5
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Starflex® GM1810BA Metallocene Linear Low Density Polyethylene, Film Extrusion Grade
LyondellBasell Starflex® GM1835CAX01 Metallocene Linear Low Density Polyethylene, Film Extrusion Grade
Total Lumicene® mPE M 3410 EP HDPE Film
Total Lumicene® mPE M5220 M Metallocene High Density Polyethylene
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene

PEQU0823 / 104179

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.