MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 50-11/AboCure 50-12 Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Information provided by Abatron, Inc.

Processing: Shelf life: 12+ months (unmixed). 100/13.5 ratio. Pot life: 500 g, 36 min. at 25°C (77°F). Exothermic Peak 265°C (510°F). Hardens in 2-24 hours at RT (faster with heat). Full cure in 1-5 weeks at RT or 1-4 hrs at 80-120°C (175-250°F).

Key Words: potting, casting, encapsulating, impregnating
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 400400
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9696
Tensile Strength, Ultimate 73.84 MPa10710 psi
Elongation at Break 7.5 %7.5 %
Flexural Yield Strength 81.56 MPa11830 psi
Flexural Modulus 2.79 GPa405 ksi
Compressive Yield Strength 98.25 MPa14250 psi
Compressive Modulus 2.10 GPa305 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.19e+16 ohm-cm1.19e+16 ohm-cm
Surface Resistance >= 1.19e+16 ohm>= 1.19e+16 ohm
Dielectric Constant  3.31
@Frequency 1e+6 Hz
3.31
@Frequency 1e+6 Hz
 3.77
@Frequency 1000 Hz
3.77
@Frequency 1000 Hz
 3.84
@Frequency 60 Hz
3.84
@Frequency 60 Hz
Dissipation Factor  0.0079
@Frequency 60 Hz
0.0079
@Frequency 60 Hz
 0.017
@Frequency 1000 Hz
0.017
@Frequency 1000 Hz
 0.028
@Frequency 1e+6 Hz
0.028
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 84.0 °C183 °FDeflection temperature; load unknown.
 
Processing PropertiesMetricEnglishComments
Pot Life 36 min36 min500 g
 
Descriptive Properties
Exotherm265°CPeak

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Devcon Zip Patch™ Epoxy
Devcon Underwater Repair Putty (UW) Epoxy
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste
Abatron AboCast/AboCure 8502-1 Epoxy

PABDS1 / 21997

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.