MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

KEP Kepital® TE-23 (FU2015) Acetal Copolymer, High toughness
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: High improvement in impact strength and flexibility. TE-23 is higher impact modified than TE-22, so is suitable for parts that high impact resistance is needed.

Information provided by KEP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Water Absorption 0.24 %0.24 %ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm0.018 in/int = 3 mm
Melt Flow 7.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.0 MPa6530 psi50 mm/min; ISO 527
Elongation at Break 86 %86 %50 mm/min; ISO 527
Elongation at Yield 12 %12 %50 mm/min; ISO 527
Flexural Strength 58.0 MPa8410 psiISO 178
Flexural Modulus 1.65 GPa239 ksiISO 178
Charpy Impact, Notched 1.45 J/cm²6.90 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C72.2 µin/in-°FISO 11359
Melting Point 165 °C329 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C169 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KEP Kepital® TE-25 (FU2025) Acetal Copolymer, High toughness
Delrin Delrin® 100ST NC010 POM-HI
Delrin Delrin® 500T NC010 POM-I
KEP Kepital® TE-22 Acetal Copolymer, High toughness
Chi Mei Polylac® PA-757 ABS

PKEP9924 / 185600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.