MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Categories: Polymer

Material Notes: CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measure 34 cSt34 cSt
Thickness 0.800 - 1.80 microns0.0315 - 0.0709 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 78.0 - 96.0 MPa11300 - 13900 psi
Elongation at Break 5.5 - 10.5 %5.5 - 10.5 %
Tensile Modulus 2.70 - 3.10 GPa392 - 450 ksi
Poissons Ratio 0.340.34
Shear Modulus 1.01 - 1.16 GPa146 - 168 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+19 ohm-cm1.00e+19 ohm-cm
Dielectric Constant 2.65
@Frequency 1.00e+9 - 2.00e+10 Hz
2.65
@Frequency 1.00e+9 - 2.00e+10 Hz
Dielectric Strength 530 kV/mm13500 kV/in
Dissipation Factor 0.000800.00080
 
Thermal PropertiesMetricEnglishComments
CTE, linear 42.0 µm/m-°C
@Temperature 20.0 °C
23.3 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg >= 350 °C>= 662 °F
Decomposition Temperature 350 °C662 °F1.7% weight loss per hour
 
Descriptive Properties
Stress on Si MPa, Min26 - 30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow CYCLOTENE™ 3022-46 Bisbenzocyclobutene (BCB) Electronic Resin
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin

PDOW1043 / 30247

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.