MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: W3T282-42"-F263; Fiber: T300 Celion

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 61.0 %61.0 %Laminate Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  541 MPa
@Temperature 177 °C
78500 psi
@Temperature 351 °F
 570 MPa
@Temperature 24.0 °C
82700 psi
@Temperature 75.2 °F
Tensile Modulus  57.7 GPa
@Temperature 177 °C
8370 ksi
@Temperature 351 °F
 60.7 GPa
@Temperature 24.0 °C
8800 ksi
@Temperature 75.2 °F
Compressive Yield Strength  575 MPa
@Temperature 71.0 °C
83400 psi
@Temperature 160 °F
 648 MPa
@Temperature 24.0 °C
94000 psi
@Temperature 75.2 °F
Shear Strength  46.0 MPa
@Temperature 177 °C
6670 psi
@Temperature 351 °F
Short Beam
 56.0 MPa
@Temperature 132 °C
8120 psi
@Temperature 270 °F
Short Beam
 72.0 MPa
@Temperature -54.0 °C
10400 psi
@Temperature -65.2 °F
Short Beam
 74.0 MPa
@Temperature 24.0 °C
10700 psi
@Temperature 75.2 °F
Short Beam
 
Descriptive Properties
Cured Thickness per Ply (cm)0.018Laminate
Dry Resin Content (%)38-42Prepreg
Flow (%)9-22

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® F155 Epoxy Resin, W3T282 Carbon Fabric
Hexcel® HexPly® F155 Epoxy Resin, F3T584 Carbon Fabric
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric
Hexcel® HexPly® F522 Epoxy Resin, F3C433 Carbon Fabric
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric

PHEXC119 / 98589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.