MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³Resin Density
 2.60 g/cc0.0939 lb/in³Fiber Density
Filler Content 35.0 %35.0 %Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 280 MPa40600 psi90º, RT, Dry; EN2561
Tensile Modulus 17.0 GPa2470 ksi90º, RT, Dry; EN2561
Shear Strength 49.7 MPa7210 psi90º, ILSS Short Beam, RT, Dry; EN2563
 55.0 MPa7980 psi0º, ILSS Short Beam, RT, Dry; EN2563
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 - 130 °C248 - 266 °FEpoxy Matrix Limit
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Cured Thickness per Ply (cm)0.015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric
Hexcel® HexPly® F185 Epoxy Resin, 120 Glass Fabric
Hexcel® HexPly® F263 Epoxy Resin, 120 Glass Fabric

PHEXC182 / 98653

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.