MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI LATILON 30-V0 Polycarbonate (PC) (UL94 V-0)  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Description: Latilon thermoplastics are polycarbonate (PC) products. The Latilons feature good mechanical characteristics and excellent toughness even at low temperatures, and good resistance to UV light. Water absorption is low, but a continuous contact with hot water above 50°C is not recommended, as resistance to hydrolysis is not sufficient. Dimensional stability is excellent. Ageing resistance is also very good when the products are free from strains. Reinforced Latilons are among the few polymers to guarantee good mechanical properties also at high temperatures; creep strength is excellent. Continuous no-load working temperature is 135°C (150°C for short periods).

Specific Notes for this Material: UL94 V0 (1.47 mm) self-extinguishing, bromine and phosphorus free; low fume optical density and toxicity; average/high viscosity; excellent surface finish.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Water Absorption 0.10 %0.10 %at 23°C; ISO 62
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inLATI
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Tensile Strength, Ultimate 64.0 MPa9280 psiISO 527
 46.0 MPa
@Temperature 120 °C
6670 psi
@Temperature 248 °F
ISO 527
 48.0 MPa
@Temperature 90.0 °C
6960 psi
@Temperature 194 °F
ISO 527
 51.0 MPa
@Temperature 60.0 °C
7400 psi
@Temperature 140 °F
ISO 527
Flexural Modulus 2.40 GPa348 ksiASTM D790
 1.70 GPa
@Temperature 120 °C
247 ksi
@Temperature 248 °F
ASTM D790
 1.80 GPa
@Temperature 90.0 °C
261 ksi
@Temperature 194 °F
ASTM D790
 2.20 GPa
@Temperature 60.0 °C
319 ksi
@Temperature 140 °F
ASTM D790
Izod Impact, Notched  1.00 J/cm
@Temperature -40.0 °C
1.87 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 1.20 J/cm
@Temperature -20.0 °C
2.25 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 7.00 J/cm
@Temperature 23.0 °C
13.1 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched  >= 30.0 J/cm²
@Temperature -20.0 °C
>= 143 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 >= 30.0 J/cm²
@Temperature -40.0 °C
>= 143 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 >= 30.0 J/cm²
@Temperature 23.0 °C
>= 143 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.0 kV/mm
@Thickness 2.00 mm
457 kV/in
@Thickness 0.0787 in
IEC 243-1
Comparative Tracking Index 200 V200 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 75.0 µm/m-°C
@Temperature 20.0 °C
41.7 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 135 °C275 °F
 150 °C302 °F
Deflection Temperature at 0.46 MPa (66 psi) 141 °C286 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °FASTM D648
Vicat Softening Point 147 °C297 °F50°C/h 50N; ISO 306
Flammability, UL94  V-2
@Thickness 0.910 mm
V-2
@Thickness 0.0358 in
 V-0
@Thickness 1.70 mm
V-0
@Thickness 0.0669 in
Oxygen Index 34 %34 %ISO 4589
Glow Wire Test  960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 695-2-1
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 300 °C518 - 572 °F
Mold Temperature 90.0 - 110 °C194 - 230 °F
Drying Temperature 120 - 130 °C248 - 266 °FTemperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourDrying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)YIEC 335
Heat Resistance - Ball Test (165°C)NIEC 335
Injection Speedhigh
Needle Burner TestY1.47 mm
 Y3.05 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 600 HB Acrylonitrile Butadiene Styrene (ABS), UL94 HB
LATI LATILON 24 Low Viscosity Polycarbonate (PC)
LATI LASTILAC AR-V0 Acrylonitrile Butadiene Styrene (ABS) (UL94 V-0 5V)
LATI LATILON 28 Polycarbonate (PC)
Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber

PLATI169 / 50167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.