MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TPI Porene® ABS-SR101 High Impact Extrusion Grade ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Poly(Acrylonitrile Butadiene Styrene); Thai Petrochemical Industry; Polymer Technology & Services, LLC (PTS)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 43.0 MPa
@Thickness 3.17 mm
6240 psi
@Thickness 0.125 in
Flexural Yield Strength 59.1 MPa
@Thickness 3.17 mm
8570 psi
@Thickness 0.125 in
Flexural Modulus 1.93 GPa
@Thickness 3.17 mm
280 ksi
@Thickness 0.125 in
Izod Impact, Notched  2.94 J/cm
@Thickness 6.35 mm
5.51 ft-lb/in
@Thickness 0.250 in
 3.58 J/cm
@Thickness 3.17 mm
6.71 ft-lb/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C198 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Stylac™ AE850 ABS Polymer, Extrusion, High Molding
Asahi Kasei Stylac™ AE510 ABS Polymer, Extrusion, High Molding
Asahi Kasei Stylac™ AE490 ABS Polymer, Extrusion, High Molding
Asahi Kasei Stylac™ A4130 ABS Polymer, Extrusion
Elix Polymers ELIX ABS E211 LNS013 Acrylonitrile Butadiene Styrene (ABS), Extrusion, Impact Grade

PLBT06 / 50502

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.