MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Pellethane® 5863-80A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Aromatic Polyether-based Thermoplastic Polyurethane (TPU)

Features: High moisture vapor transmission. Good low temperature properties and elasticity.

Process: Extrusion and Injection Molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Water Vapor Transmission  650 g/m²/day
@Temperature 25.0 °C
41.9 g/100 in²/day
@Temperature 77.0 °F
upright cup, 50% RH; ASTM E96B
 6500 g/m²/day
@Temperature 38.0 °C
419 g/100 in²/day
@Temperature 100 °F
Mocon, 90% RH; ASTM D6701
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength, Ultimate 31.0 MPa4500 psiASTM D412
Elongation at Break 700 %700 %ASTM D412
100% Modulus 4.50 MPa
@Strain 100 %
653 psi
@Strain 100 %
ASTM D412
300% Modulus 8.30 MPa
@Strain 300 %
1200 psi
@Strain 300 %
ASTM D412
Tear Strength 17.5 kN/m99.9 pliTrouser; ASTM D470
Graves Tear Strength 61.4 kN/m350 plidie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 60
@Load 1.00 kg
60
@Load 2.20 lb
H-18; ASTM D3389
Tensile Set 10 %
@Temperature 200 °C
10 %
@Temperature 392 °F
ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 °C275 °F
 275 °C527 °FKofler
Glass Transition Temp, Tg -37.0 °C-34.6 °F
 
Processing PropertiesMetricEnglishComments
Zone 1 171 °C340 °F
Zone 2 177 °C351 °F
Zone 3 182 °C360 °F
Zone 4 188 °C370 °F
Adapter Temperature 193 °C379 °F5
Die Temperature 193 °C379 °F
 193 °C379 °F2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Pellethane® 2363-80A TPU
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Lubrizol LifeSciences Pellethane® 2363-65D TPU
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based

PLUBR9033 / 203600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.