Product description: Grivory G 25 is a very high viscous amorphous copolyamide. It is suitable for injection stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of coextruded blown film and mono-or coextruded cast film and coextrusion of tubes. Grivory G 25 is also used as an additive for polyamide 6 and different copolyamides to improve film properties. The key properties of Grivory G 25 are:- High transparency and high surface gloss
- Very good chemical resistance
- Very good abrasion resistance
- Excellent flavor and aroma barrier
- Improved gas and aroma barrier at elevated relative humidity
- Low transmission of UV radiation
Application examples: Barrier layer for mono- or coextruded rigid packaging (EBM or ISBM bottles), barrier tubes, barrier layer in multilayer films for flexible food and cosmetics packaging, barrier layer modifier for flexible meat/cheese or other food packaging.Information provided by EMS Grivory |