MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ArcelorMittal H 260 Solid solution steel, Cold rolled
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Available in the following: uncoated (HC260P) and electrogalvanized (HC260P+ZE)

Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These steels are hardened by phosphorous in solid solution in the ferrite. Their combination of mechanical strength and drawability makes these grades suitable for numerous applications. They are particularly recommended for structural and reinforcement parts requiring good fatigue and impact strength (longitudinal beams, cross members, B-pillars, etc.). Solid solution steels are killed aluminum grades with lower drawing quality than the IF range of steels. The ArcelorMittal range of continuous hot dip galvanized (Extragal®/Galvannealed) steels is described under interstitial-free steels.

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 380 - 440 MPa55100 - 63800 psi
Tensile Strength, Yield 260 - 320 MPa37700 - 46400 psi
Elongation at Break >= 29 %>= 29 %L0=80 mm, th<3 mm
Fatigue Strength  <= 320 MPa
@# of Cycles 2.00e+6
<= 46400 psi
@# of Cycles 2.00e+6
 <= 320 MPa
@# of Cycles 1.00e+7
<= 46400 psi
@# of Cycles 1.00e+7
 <= 350 MPa
@# of Cycles 100000
<= 50800 psi
@# of Cycles 100000
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Iron, Fe >= 98.74 %>= 98.74 %as balance
Manganese, Mn <= 0.70 %<= 0.70 %
Silicon, Si <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ArcelorMittal HSLA 260 High strength low alloy steel for cold forming, Cold Rolled
AISI Type 651 (19-9) Stainless Steel cold rolled and stress relieved, 35 HRC hardness
ArcelorMittal 260 BH Bake hardening steel, Cold rolled
AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1022 Steel, cold rolled, 25 mm (1 in.) round

NARCE059 / 159967

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.