MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese SO.F.TER Styrofor® HI-V0 Self Extinguishing Polystyrene, Flame Resistant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant; Polystyrene (PS)

Material Notes: Very good flow and good impact resistance. Polystyrene based compound. These compounds are used mainly in the automotive and household industry to manufacture outer casings and protection guards, in the furniture sector to manufacture chairs, for the production of footwear, and for the production of sport articles such as helmets, ski boots, and roller blades.

Information provided by SO.F.TER. Spa

Key Words: Softer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D1505, ISO 1183
Water Absorption 0.060 %0.060 %24 hours; ASTM D570, ISO 62
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Index of Compound 15 g/10 min15 g/10 minASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.0 MPa4350 psiASTM D638, ISO 527
Elongation at Break 20 %20 %ASTM D638, ISO 527
Flexural Modulus 2.30 GPa334 ksiASTM D790, ISO 178
Izod Impact, Unnotched 0.800 J/cm1.50 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 250 V250 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 75.0 °C167 °FIEC 335
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FASTM D648, ISO 75
Vicat Softening Point 90.0 °C194 °F49N/50; ASTM D1525, ISO 306
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Oxygen Index 21 %21 %ASTM D2863
Glow Wire Test 960 °C1760 °FIEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 160 - 180 °C320 - 356 °FCylinder Temperature
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 60.0 °C140 °F
Dry Time 2 hour2 hour
 
Descriptive Properties
Needle FlameOKIEC 695-2-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hannam Chemical Hanalac 740 ABS, Super High Impact Grade
Covestro Apec® FR1892 High-Heat Polycarbonate
Envalior TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Evonik Europlex® 99510 Film Transparent Polycarbonate Based Film
Teknor Apex Synres® PP HFR005 Polypropylene

PSOFT35 / 67909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.