MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Y-TZP Y2O3 Stabilized Zirconia
Categories: Ceramic; Oxide

Material Notes: Ultra fine grain, with very high mechanical strength, plus superior corrosion and abrasion resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.00 g/cc0.217 lb/in³Fired
Porosity 0.00 %0.00 %Apparent, fully dense
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 45 N 8080
Vickers Microhardness 1250012500MPa, at Hv 0.5kg
Modulus of Elasticity 200 GPa
@Temperature 20.0 °C
29000 ksi
@Temperature 68.0 °F
Flexural Strength 800 - 900 MPa
@Temperature 20.0 °C
116000 - 131000 psi
@Temperature 68.0 °F
3-point
Fracture Toughness 10.0 MPa-m½9.10 ksi-in½
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.00 - 10.6 µm/m-°C
@Temperature 20.0 °C
5.00 - 5.89 µin/in-°F
@Temperature 68.0 °F
 9.00 - 10.9 µm/m-°C
@Temperature 800 °C
5.00 - 6.06 µin/in-°F
@Temperature 1470 °F
Specific Heat Capacity 0.610 J/g-°C0.146 BTU/lb-°F
Thermal Conductivity 2.90 W/m-K
@Temperature 20.0 °C
20.1 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 200 °C392 °F
 
Descriptive Properties
Thermal Downshock260Change in °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade
China-Yixing Longly Refractories Zirconia Ceramics
AK Steel 316 Austenitic Stainless steel
CoorsTek ZDY Yttria Fully Stabilized Zirconia
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5%

CMORG32 / 90410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.