MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA334000 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability.

Regulatory Status
NA 334-000 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.

Processing Techniques
NA 334-000 is specifically designed to provide outstanding drawdown at maximum outputs. The melt strength properties of this resin result in excellent bubble stability. This resin can be processes over a wide range of temperatures; however, recommended conditions are melt temperatures between 300°-330°F and a blow-up ratio between 2.0-2.5:1. Using proper techniques and equipment, drawdown to 0.25 mil is feasible at commercial production rates. Specific recommendations for processing NA 334-000 can only be made when the processing conditions, equipment and end use are known.

Other Information
No slip, no antiblock.

Physical Properties
These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron)

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Thickness 31.8 microns1.25 mil2.2:1 BUR
Melt Flow 6.0 g/10 min6.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 300 %300 %ASTM D882
Film Elongation at Break, TD 450 %450 %ASTM D882
Dart Drop Test 65.0 g0.143 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 15.2 MPa2200 psiASTM D882
Film Tensile Strength at Break, TD 13.8 MPa2000 psiASTM D882
1% Secant Modulus, MD 138 MPa20000 psiASTM D882
1% Secant Modulus, TD 159 MPa23000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Gloss 50 %50 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 163 °C325 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman PE1059 Film Extrusion Polyethylene
Huntsman PE5050 Extrusion Coating Polyethylene
ExxonMobil LD 6520.BA Low Density Polyethylene Resin
Huntsman PE2030 Injection Molding Polyethylene
Huntsman PE5030 Extrusion Coating Polyethylene

PEQU0477 / 36924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.