MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec Alunit® HS Aluminum Nitride
Categories: Ceramic; Nitride

Material Notes: Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its electrical and mechanical characteristics are similar to aluminum oxide. Alunit® HS is non-toxic and environmentally compatible, presenting no disposal problems. Alunit® HS substrates come in a variety of surface finishes: as fired, as fired superior, ground, or polished. They can be manufactured by using tape casting, dry pressing, lasering, or metallizing. Typical applications include: power electronics, IGBT modules, telecommunications, cooling devices, DCB (Direct Copper Bonding), and LEDs.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.33 g/cc0.120 lb/in³ASTM-C20
Water Absorption 0.00 %0.00 %ASTM-C373
Particle Size 4.0 - 5.0 µm4.0 - 5.0 µmMedium Grain (d50)
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 320 GPa46400 ksiASTM-F417
Flexural Strength 420 MPa60900 psiBending Strength; 4-Point Method (40x4x3 mm³); ASTM-F417
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM-D257
Dielectric Constant 9.0
@Frequency 1e+6 Hz
9.0
@Frequency 1e+6 Hz
ASTM-C150
Dielectric Breakdown >= 16000 V
@Thickness 1.00 mm
>= 16000 V
@Thickness 0.0394 in
ASTM-D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.70 µm/m-°C
@Temperature 20.0 - 300 °C
2.61 µin/in-°F
@Temperature 68.0 - 572 °F
ASTM-C372
 5.20 µm/m-°C
@Temperature 20.0 - 600 °C
2.89 µin/in-°F
@Temperature 68.0 - 1110 °F
ASTM-C372
 5.60 µm/m-°C
@Temperature 20.0 - 1000 °C
3.11 µin/in-°F
@Temperature 68.0 - 1830 °F
ASTM-C372
Specific Heat Capacity 0.738 J/g-°C0.176 BTU/lb-°F
Thermal Conductivity 170 W/m-K1180 BTU-in/hr-ft²-°FASTM-C408
 
Descriptive Properties
ColorTranslucent Medium Gray
Ra = Arithmetic Mean Roughness Value (µm)Profilometer (cutoff 0.8 mm); DIN ISO 4287

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Alunit® Aluminum Nitride
CeramTec Rubalit® 708S Alumina, 96%
CeramTec CeramCool® Alunit® Aluminum Nitride
Ceradyne Ceralloy® 1370DP Aluminum Nitride
H.C. Starck Grade C Aluminum Nitride AIN

CCERA946 / 107546

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.