MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton 601 Chain Drive Pin & Bushing Lubricant
Categories: Fluid; Lubricant

Material Notes: Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was specially formulated to penetrate between the close clearance of chain drive bushings and pins to provide critical lubrication after penetrating close metal to metal tolerance, 601 Chain Drive Pin & Bushing Lubricant provides a long lasting nondrying film which effectively lubricates metal surfaces so they run smoothly with far less wear.

Features:

  • Rapid Penetration
  • Excellent Hydrodynamic Lubrication
  • Noticeably Extends Chain Life
  • NSF H2- Registration number 133979 (bulk) and 133927 (aerosol)

Applications for 601 Chain Drive Pin & Bushing Lubricant can be found in every industry in both the production and maintenance areas. Use on any chain drive for assembly lines, conveyers, packaging equipment, hoist chains, link and roller assemblies, forklift trucks, tractors, machinery, chain saws and for any application requiring a high grade light oil. Used on robotic equipment, the product works extremely well both as a lubricant and as an anti-slag coating, allowing easy removal of excess weld spatter.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/cc
Kinematic Viscosity at 40°C (104°F) 22 cSt22 cStASTM D445, DIN 51 561
Kinematic Viscosity at 100°C (212°F) 4.0 cSt4.0 cStASTM D445, DIN 51 561
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 160 kg353 lb (mass)ASTM D2596, DIN 51 350/4
Four Ball Wear 0.500 mm
@Temperature 75.0 °C,
Time 3600 sec
0.0197 in
@Temperature 167 °F,
Time 1.00 hour
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350/5
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -23.0 °C-9.40 °F
Pour Point -25.0 °C-13.0 °FASTM D97, DIN 51 350
Flash Point 127 °C261 °FASTM D93, DIN 51 755
 
Descriptive Properties
AppearanceClear, Amber Liquid
Pin & Vee Block<750 kgFailure Load, ASTM D3233
 0.06Coefficient of Friction, ASTM D3233
 3.2 N.mTorque, ASTM D3233

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018
Cheng Yu Plastic ML1210 PC/PTFE, 10% Glass
ASTM A439 Austenitic Ductile Iron type D4
Akzo Nobel Expancel® 820 DU 40 Dry unexpanded microspheres
Akzo Nobel Expancel® 551 DU 40 Dry unexpanded microspheres

PPTCHS076 / 138188

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.