MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: High Toughness, Heavy Section Weldable Alloy

A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited for applications in marine environments where toughness and corrosion resistance are essential. The alloy was developed jointly with the US Navy, and has been selected as the material of choice for a submarine application.

Data provided by TIMET.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.43 g/cc0.160 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 862 MPa125000 psiTypical
Tensile Strength, Yield 758 MPa
@Strain 0.2 %
110000 psi
@Strain 0.2 %
Typical
Elongation at Break 15 %15 %Typical
Reduction of Area 30 %30 %
Modulus of Elasticity 107 - 114 GPa15500 - 16500 ksiTypical
Bend Radius, Minimum 5.0 t5.0 tTypical; on 0.078 in (2 mm) sheet
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.000153 ohm-cm
@Temperature 24.0 °C
0.000153 ohm-cm
@Temperature 75.2 °F
 0.000164 ohm-cm
@Temperature 152 °C
0.000164 ohm-cm
@Temperature 306 °F
 0.000173 ohm-cm
@Temperature 301 °C
0.000173 ohm-cm
@Temperature 574 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.20 µm/m-°C
@Temperature 50.0 °C
4.56 µin/in-°F
@Temperature 122 °F
 9.30 µm/m-°C
@Temperature 250 °C
5.17 µin/in-°F
@Temperature 482 °F
Specific Heat Capacity  0.533 J/g-°C
@Temperature 24.0 °C
0.127 BTU/lb-°F
@Temperature 75.2 °F
 0.572 J/g-°C
@Temperature 146 °C
0.137 BTU/lb-°F
@Temperature 295 °F
 0.613 J/g-°C
@Temperature 300 °C
0.147 BTU/lb-°F
@Temperature 572 °F
Thermal Conductivity  7.50 W/m-K
@Temperature 24.0 °C
52.0 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
 8.87 W/m-K
@Temperature 146 °C
61.6 BTU-in/hr-ft²-°F
@Temperature 295 °F
 10.7 W/m-K
@Temperature 300 °C
74.3 BTU-in/hr-ft²-°F
@Temperature 572 °F
Beta Transus 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 4.5 - 5.5 %4.5 - 5.5 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.25 %<= 0.25 %
Molybdenum, Mo 0.60 - 1.2 %0.60 - 1.2 %
Nitrogen, N <= 0.030 %<= 0.030 %
Oxygen, O <= 0.11 %<= 0.11 %
Silicon, Si 0.060 - 0.14 %0.060 - 0.14 %
Tin, Sn 0.60 - 1.4 %0.60 - 1.4 %
Titanium, Ti 88.5 - 93 %88.5 - 93 %Calculated as remainder
Vanadium, V 0.60 - 1.4 %0.60 - 1.4 %
Zirconium, Zr 0.60 - 1.4 %0.60 - 1.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-6Al-2Nb-1Ta-0.8Mo (Ti-621/0.8), Alpha-Annealed
Titanium Ti-8Al-1Mo-1V (Ti-8-1-1), Beta Solution Treated
TIMET TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si), Beta Anneal + 1400°F
ATI Allvac® 6-2-4-2 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age
TIMET TIMETAL® 3-2.5-0.05Pd Titanium Alloy

NTIME5111 / 19302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.