Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivory GC-4H is used for injection molding of high performance technical parts, exhibiting exceptional characteristics even after moisture absorption:- very high stiffness and strength
- dimensional stability, low warpage
- good chemical resistance
- electrical and thermal conductive
- favorable abrasion and wear properties
- low weight
Grivory GC-4H is suitable in the application fields of:- Electro /Electronics
- Safety technology
- Mechanical engineering
Grivory GC-4H is only available in black.Information provided by EMS Grivory |