MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TPI Porene® ABS-SP-100 Super High Impact ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Poly(Acrylonitrile Butadiene Styrene); Thai Petrochemical Industry; Polymer Technology & Services, LLC (PTS)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Melt Flow 18 g/10 min
@Load 10.0 kg,
Temperature 220 °C
18 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength, Yield 44.1 MPa
@Thickness 3.17 mm
6400 psi
@Thickness 0.125 in
Flexural Yield Strength 63.4 MPa
@Thickness 3.17 mm
9200 psi
@Thickness 0.125 in
Flexural Modulus 2.15 GPa
@Thickness 3.17 mm
312 ksi
@Thickness 0.125 in
Izod Impact, Notched  3.31 J/cm
@Thickness 6.35 mm
6.20 ft-lb/in
@Thickness 0.250 in
 4.00 J/cm
@Thickness 3.17 mm
7.49 ft-lb/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FASTM D648
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 193 °C380 °F
Middle Barrel Temperature 216 °C420 °F
Front Barrel Temperature 227 °C440 °F
Melt Temperature 232 - 260 °C450 - 500 °FNozzle temp not greater than stock
Mold Temperature 48.9 - 65.6 °C120 - 150 °F
Drying Temperature 87.8 - 93.3 °C190 - 200 °F
Dry Time 2 - 24 hour2 - 24 hour
Injection Pressure 68.9 - 82.7 MPa10000 - 12000 psi
Back Pressure 0.689 MPa100 psi
Screw Speed 50 - 60 rpm50 - 60 rpm
 
Descriptive Properties
Injection Fill SpeedSlow to Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
IRPC Polimaxx Porene SP100 Acrylonitrile Butadiene Styrene
Lotte Advanced Materials Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
A. Schulman Diamond ABS 9401 Injection Molding Grade, Ultra High Impact
Chi Mei Wonderloy® PC-510 PC/ABS Alloy - Flame Retardant

PLBT05 / 50501

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.