MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® A-601C with 60 MT Black Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Fully precompounded for O-ring curative level
  • Improved processing for a high viscosity polymer with improved mold flow, easier mold release, and less mold fouling
  • Excellent scorch safety
  • Excellent physical properties for improved compression set resistance

Applications

  • Compression molding of O-rings, gaskets, and other sealing devices
  • Applications where a higher polymer viscosity is needed for molding operations. Can be used to modify viscosity of other types of Viton®.
  • Can be formulated to meet FKM specifications Mil-R-83248C and AMS 7276E.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 144
@Temperature 121 °C
144
@Temperature 250 °F
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8989ASTM D2240
Tensile Strength at Break 16.6 MPa2410 psiASTM D412
Elongation at Break 159 %159 %ASTM D412
100% Modulus 11.7 MPa
@Strain 100 %
1700 psi
@Strain 100 %
ASTM D412
Compression Set  9.0 %
@Temperature 23.0 °C,
Time 252000 sec
9.0 %
@Temperature 73.4 °F,
Time 70.0 hour
O-Rings; ASTM D395B
 11 %
@Temperature 200 °C,
Time 79200 sec
11 %
@Temperature 392 °F,
Time 22.0 hour
O-Rings; ASTM D395B
 14 %
@Temperature 200 °C,
Time 79200 sec
14 %
@Temperature 392 °F,
Time 22.0 hour
O-Rings; ASTM D395B
 20 %
@Temperature 200 °C,
Time 252000 sec
20 %
@Temperature 392 °F,
Time 70.0 hour
O-Rings; ASTM D395B
 29 %
@Temperature 200 °C,
Time 605000 sec
29 %
@Temperature 392 °F,
Time 168 hour
O-Rings; ASTM D395B
 39 %
@Temperature 232 °C,
Time 252000 sec
39 %
@Temperature 450 °F,
Time 70.0 hour
O-Rings; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature  177 °C
@Time 601 sec
351 °F
@Time 0.167 hour
Slab Cure
 232 °C
@Time 86400 sec
450 °F
@Time 24.0 hour
Postcure
 
Descriptive Properties
Formulation as Tested100A-601C
 3MgO
 6Ca(OH)2
 60MT Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® A-601C with MT Black Fluoroelastomer Compound
Chemours Viton® GLT-600S with 5-MT Black Fluoroelastomer Compound
Chemours Viton® GF-600S with 3phr, 802-40KE Fluoroelastomer Compound
Chemours Viton® GBLT-600S with 10022 Fluoroelastomer Compound
Chemours Viton® GBLT-600S Fluoroelastomer Compound

PDVC9928 / 170569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.