MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iran Petrochemical (PCC) PC 5970 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Suitable for injection molding

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Melt Flow 59.1 - 70 g/10 min
@Load 1.20 kg,
Temperature 300 °C
59.1 - 70 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness >= 103 MPa>= 14900 psiDIN 53456
Tensile Stress 55.0 - 70.0 MPa7980 - 10200 psiASTM D638
Tensile Strength, Yield >= 60.0 MPa>= 8700 psiASTM D638
Elongation at Break >= 50 %>= 50 %ASTM D638
Modulus of Elasticity 2.20 - 2.40 GPa319 - 348 ksiASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.8 - 3.1
@Frequency 1e+6 Hz
2.8 - 3.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength >= 20.0 kV/mm
@Frequency 50 Hz
>= 508 kV/in
@Frequency 50 Hz
ASTM D149
Dielectric Loss Index  0.00080 - 0.0010
@Frequency 5e+7 Hz
0.00080 - 0.0010
@Frequency 5e+7 Hz
ASTM D150
 0.0080 - 0.011
@Frequency 1e+6 Hz
0.0080 - 0.011
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 140 - 150 °C284 - 302 °F50 N, 50°C/h; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 80 %
@Thickness 2.00 mm
>= 80 %
@Thickness 0.0787 in
ASTM D1003
 
Descriptive Properties
Solvent Content, ppm< 500GC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) PC 1218 Polycarbonate
Iran Petrochemical (PCC) PC 1822 Polycarbonate
Iran Petrochemical (PCC) PC 2230 Polycarbonate
Iran Petrochemical (PCC) PC 3038 Polycarbonate
Iran Petrochemical (PCC) PC 3859 Polycarbonate

PIPC370 / 149803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.