MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NAECO® ELKONIUM® 28 Silver Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: ELKONIUM® 28, a silver-manganese alloy, was developed by CMW specifically for the control of the transfer of contact material in low voltage DC applications. It is used as a positive contact operating against a CMW D582F (silver graphite, see Series 300) negative contact in vibrating contact automobile voltage regulators.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.0 g/cc0.397 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 15T 6868annealed
 7575cold worked
Tensile Strength, Ultimate 207 MPa30000 psiannealed
 276 MPa40000 psicold worked
Elongation at Break 5.0 %5.0 %cold worked
 32 %32 %annealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000172 ohm-cm0.0000172 ohm-cm10 % IACS
 
Component Elements PropertiesMetricEnglishComments
Manganese, Mn 5.0 %5.0 %
Silver, Ag 95 %95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
CMW® D1058 Silver Graphite Contact Material
CMW® D57F Silver Iron Contact Material
CMW® D58 Silver Graphite Contact Material
CMW® ELKONIUM 28 Silver Alloy

NCMV891 / 192377

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.