MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® 2805 Polycarbonate, Injection Grade
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: MVR (300 °C/1.2 kg) 9.0 cm³/10 min; general purpose; medium viscosity; easy release; injection molding - melt temperature 280 - 320 °C; available in transparent, translucent and opaque colors

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³pellets; ISO 60
Density 1.20 g/cc0.0434 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.12 %0.12 %50% RH; ISO 62
Water Absorption at Saturation 0.35 %0.35 %ISO 62
Water Vapor Transmission 15.0 g/m²/day0.966 g/100 in²/dayISO 15106-1
Oxygen Transmission 650 cc-mm/m²-24hr-atm1650 cc-mil/100 in²-24hr-atmcm³/(m²·24 h·bar), 100 µm film; b.o. ISO 2556
 2760 cc-mm/m²-24hr-atm7010 cc-mil/100 in²-24hr-atmcm³/(m²·24 h·bar), 25.4 µm (1 mil) film; b.o. ISO 2556
Nitrogen Transmission 120 cc-mm/m²-24hr-atm305 cc-mil/100 in²-24hr-atmcm³/(m²·24 h·bar), 100 µm film; b.o. ISO 2556
 510 cc-mm/m²-24hr-atm1300 cc-mil/100 in²-24hr-atmcm³/(m²·24 h·bar), 25.4 µm (1 mil) film; b.o. ISO 2556
Carbon Dioxide Transmission 3800 cc-mm/m²-24hr-atm9650 cc-mil/100 in²-24hr-atmcm³/(m²·24 h·bar), 100 µm film; b.o. ISO 2556
 16900 cc-mm/m²-24hr-atm42900 cc-mil/100 in²-24hr-atmcm³/(m²·24 h·bar), 25.4 µm (1 mil) film; b.o. ISO 2556
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inb.o. ISO 2577
Linear Mold Shrinkage, Flow 0.0065 cm/cm0.0065 in/in60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  24000 N
@Temperature 23.0 °C
5400 lb (f)
@Temperature 73.4 °F
ISO 6603-2
 28000 N
@Temperature -30.0 °C
6300 lb (f)
@Temperature -22.0 °F
ISO 6603-2
Ball Indentation Hardness 115 MPa16700 psiISO 2039-1
Tensile Strength at Break 70.0 MPa10200 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 66.0 MPa9570 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %Nominal, 50 mm/min; ISO 527-1,-2
Elongation at Yield 6.2 %6.2 %50 mm/min; ISO 527-1,-2
 130 %130 %50 mm/min; b.o. ISO 527-1,-2
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 97.0 MPa14100 psi2 mm/min; ISO 178
Flexural Yield Strength 73.0 MPa10600 psiat 3.5% strain; 2 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2 mm/min; ISO 178
Flexural Strain at Yield 7.1 %7.1 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  15.0 kJ/m²
@Thickness 76.2 mm,
Temperature -30.0 °C
7.14 ft-lb/in²
@Thickness 3.00 in,
Temperature -22.0 °F
complete break; ISO 7391/b.o. ISO 180-A
 70.0 kJ/m²
@Thickness 76.2 mm,
Temperature 23.0 °C
33.3 ft-lb/in²
@Thickness 3.00 in,
Temperature 73.4 °F
partial break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
 NB
@Temperature -60.0 °C
NB
@Temperature -76.0 °F
ISO 179-1eU
Charpy Impact, Notched  1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
3 mm, complete break; ISO 7391/b.o. ISO 179-1eA
 7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
3 mm, partial break; ISO 7391/b.o. ISO 179-1eA
Puncture Energy  81.3 J
@Temperature 23.0 °C
60.0 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 88.1 J
@Temperature -30.0 °C
65.0 ft-lb
@Temperature -22.0 °F
ISO 6603-2
Tensile Creep Modulus, 1 hour 2200 MPa319000 psiISO 889-1
Tensile Creep Modulus, 1000 hours 1900 MPa276000 psiv
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 600993
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm864 kV/in1 mm; IEC 60243-1
Dissipation Factor  0.00050
@Frequency 100 Hz
0.00050
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VCTI M; Solution B; IEC 60112
 250 V250 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 136 °C277 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 137 °C279 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FISO 75-1,-2
Vicat Softening Point 144 °C291 °F50 N, 50°C/h; ISO 306
 146 °C295 °F50 N, 120°C/h; ISO 306
Glass Transition Temp, Tg 145 °C293 °FISO 11357-1,-2
UL RTI, Electrical 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
Flammability, UL94  HB
@Thickness 2.50 mm
HB
@Thickness 0.0984 in
 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
Flash Point 480 °C896 °Fignition; ASTM D1929
 550 °C1020 °Fself ignition; ASTM D1929
Oxygen Index 28 %28 %Method A; ISO 4589-2
Glow Wire Test  750 °C
@Thickness 1.50 mm
1380 °F
@Thickness 0.0591 in
b.o. EDF HN60 E.02
 750 °C
@Thickness 3.00 mm
1380 °F
@Thickness 0.118 in
b.o. EDF HN60 E.02
Glow Wire Ignition Temperature  875 °C
@Thickness 0.750 mm
1610 °F
@Thickness 0.0295 in
IEC 60695-2-13
 875 °C
@Thickness 1.00 mm
1610 °F
@Thickness 0.0394 in
IEC 60695-2-13
 875 °C
@Thickness 1.50 mm
1610 °F
@Thickness 0.0591 in
IEC 60695-2-13
 900 °C
@Thickness 3.00 mm
1650 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  850 °C
@Thickness 0.750 mm
1560 °F
@Thickness 0.0295 in
IEC 60695-2-12
 850 °C
@Thickness 1.50 mm
1560 °F
@Thickness 0.0591 in
IEC 60695-2-12
 930 °C
@Thickness 3.00 mm
1710 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ISO 489
Haze <= 0.80 %
@Thickness 3.20 mm
<= 0.80 %
@Thickness 0.126 in
ISO 14782
Transmission, Visible  87 %
@Thickness 4.00 mm
87 %
@Thickness 0.157 in
ISO 13468-2
 88 %
@Thickness 3.00 mm
88 %
@Thickness 0.118 in
ISO 13468-2
 89 %
@Thickness 1.00 mm
89 %
@Thickness 0.0394 in
ISO 13468-2
 89 %
@Thickness 2.00 mm
89 %
@Thickness 0.0787 in
ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 °C572 °FInjection; ISO 294
Mold Temperature 80.0 °C176 °FInjection; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
Electrolytic corrosionA1IEC 60426
Needle flame test10 sMethod K, 3 mm; IEC 60695-11-5
 120 sMethod F, 3 mm; IEC 60695-11-5
 5 sMethod K, 2 mm; IEC 60695-11-5
 5sMethod K, 1.5 mm; IEC 60695-11-5
 60 sMethod F, 1.5 mm; IEC 60695-11-5
 60 sMethod F, 2 mm; IEC 60695-11-5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2405 Polycarbonate, Injection Grade
Covestro Makrolon® 2807 Polycarbonate, Injection Grade
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin
Covestro Makrolon® 2605 Polycarbonate, Injection Grade

PBA436 / 26937

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.