MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Thread Compound
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Texaco Thread Compound delivers value through:
  • Ability to meet API requirements for high-pressure thread compounds.
  • Galling prevention — Prevents galling in threaded connections. Joints are easier to break.
  • Excellent sealing properties at high temperatures and pressures.
  • Water absorption resistance
  • Ease of application by brush.
  • Environmental friendliness — Contains no lead or zinc.

Texaco Thread Compound is a lithium grease designed especially for casing and tubing connections in highpressure oil well service, or wherever unusually severe conditions are encountered.

Texaco Thread Compound contains copper flake, graphite, and other extreme pressure and antiwear additives

Texaco Thread Compound meets the performance requirements of API Recommended Practice 5A3, First Edition, October 1, 1996, "Recommended Practice on Thread Compounds for Casing, Tubing and Line Pipe."

This grease has superior lubrication qualities to prevent galling in threaded connections during joint makeup, and reduces torque requirements in breaking joints.

Its sealing properties will prevent leakage at temperatures as high as 149°C (300°F), while the quality and quantity of inert fillers prevent leakage of API round thread casing and tubing joints under pressure as high as 10,000 psi.

It has outstanding resistance to water absorption and is readily applied by brush to pipe joints, even in cold weather.

Texaco Thread Compound is used for API 8 round thread casings, buttress thread casings, tubing connections, and line pipes. It should not be used in rotary shoulder connections.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 222366; MSDS Number: 8994

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 4545Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 649 SUS649 SUSSee Note 3.
Saybolt Viscosity at 210°F 63 SUS63 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 140 cSt140 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 11.1 cSt11.1 cStSee Note 3.
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 325325Unworked, 25°C (77°F)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FSee Note 2.
Minimum Service Temperature, Air -15.0 °C5.00 °FSee Note 1.
Flash Point 196 °C385 °FSee Note 3.
Dropping Point 177 °C351 °F
 
Descriptive Properties
ColorBlack-Copper
TextureButtery
Thickener, %3Lithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Ramar® Diesel XDO SAE Grade 40
Phillips 66 Ecoterra® ISO Grade 150 Paper Machine Oil
NuSil EPM-2401 Silicone, Thermal Interface Material (TIM): Grease
ChevronTexaco 13 SG Diesel Engine Oil
Chesterton 989 Release Compound

WTEXA278 / 77157

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.