MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Features:
  • High heat resistance
  • Good chemical resistance
  • High impact strength
  • Excellent flow characteristics

Applications:

  • Automotive interior trim applications
  • Automotive consoles
  • Structural Housings

Information provided by Nova Chemicals

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccISO 1183
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inISO 2577
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 43.0 MPa6240 psiISO 527-2
Elongation at Break 8.0 %8.0 %ISO 527-2
Tensile Modulus 3.00 GPa435 ksiISO 527-2
Flexural Strength 87.0 MPa12600 psiISO 178
Flexural Modulus 3.20 GPa464 ksiISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²0.952 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 20.0 °C
40.0 µin/in-°F
@Temperature 68.0 °F
NOVA Chemicals Laboratory Procedure
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
@Diameter 4.00 mm
208 °F
@Diameter 0.157 in
Unannealed; bar; ISO 75-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 260 °C351 - 500 °FProfile temperatures
Melt Temperature 204 - 260 °C399 - 500 °Fair purge at equilibrium conditions
Mold Temperature 43.0 - 60.0 °C109 - 140 °FCore surface temp. at equilibrium
 54.0 - 71.0 °C129 - 160 °FCavity surface temp. at equilibrium
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiTypically 50 psi
Screw Speed 40 - 80 rpm40 - 80 rpm
 
Descriptive Properties
Injection Speedmedium-fastTypically fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
Ineos Nova 1204 High Heat Crystal Polystyrene
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 150 Gauge
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 150 Gauge
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 150 Gauge

PNOV947 / 54893

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.